Halogen Free Transparent No Clean Flux Liquid For Soldering 4.5 Medium Solid Content
Contact me for free samples and coupons.
Whatsapp:0086 18588475571
Wechat: 0086 18588475571
Skype: sales10@aixton.com
If you have any concern, we provide 24-hour online help.
xProduct Name | No-clean Liquid Flux | Appearance Characteristics | Colorless, Clear And Transparent |
---|---|---|---|
Advantage | Highly Active | Solid Content (w/w)% | 4.5±0.5 |
Specific Gravity (g/ml) | 0.805±0.008 | Closed Flash Point | 13℃ |
Recommended Thinner | X-C Thinner | Cl- Content (W/W)% | Not Detected |
High Light | transparent no clean flux liquid,no clean flux liquid 4.5 solid,flux liquid for soldering |
Colorless transparent and environmentally friendly flux No-clean liquid flux Medium solid flux
1. Introduction
◇ TUOPU X-5 is a medium-solid content (4.5% solid content), halogen-free, high-activity no-clean flux. It can be used in foaming, spraying and other forms.
2.storage method
◇ Store in a cool, dry, well-ventilated place or a dangerous goods warehouse that cannot be directly exposed to sunlight.
◇ The work area should have a "No Pyrotechnics" sign.
◇ The storage area should be clearly marked and allow designated or trained personnel to enter.
◇ There may still be residues in the empty barrels and pipelines, and heat treatment must be carried out before cleaning.
◇ Use a ventilation system that does not produce sparks.
◇ Ensure that the packaging is in good condition to avoid the accumulation and damage of the container.
◇ This product is packaged in plastic barrels with a storage period of one year. It is transported and packaged as dangerous goods.
3. Technical indicators
Parameter | Typical Value |
Appearance characteristics | colorless, clear and transparent |
Solid content (w/w)% | 4.5±0.5 |
Specific gravity (g/ml) | 0.805±0.008 |
Cl- content (W/W)% | not detected |
Closed flash point | 13℃ |
Advantage | Highly active |
Acid value (mg KOH/g) | 21±3 |
Insulation resistance (85℃/85%RH) | >1×108Ω |
Silver Chromate Paper Test | Pass |
Storage time | 12 months |
4.Common tin point problems and treatment
Cause of defect | 1 | 2 | 3 | 4 | 5 | 6 | 7 | 8 | 9 | 10 |
Missing | √ | √ | √ | |||||||
Duoxi Webbing | √ | √ | √ | √ | √ | |||||
Tin Cave Viods | √ | |||||||||
Pingoles | √ | √ | ||||||||
Lcicles | √ | √ | √ | √ | √ | √ | √ | |||
Coarse tin Graing | √ | |||||||||
Bridging | √ | √ | √ | √ | ||||||
Balling | √ | √ | √ | √ | √ | |||||
Short circuit Shorts | √ | √ | √ |
Note: √ represents the possible cause
1. The flux is in poor contact with the bottom plate; the contact angle of the bottom plate solder is improper
2. The flux density is too high or too low
3. The speed of the conveyor belt is too fast or too slow. If it is too fast, it will be sharp and shiny; if it is too slow, it will be slightly round and thick.
4. Too much anti-oxidation oil or deterioration in the tin furnace
5. The preheating temperature is too high or too low
6. The temperature of the tin furnace is too high or too low, if it is too high, it will be slightly round and stubby, and if it is too low, it will be sharp and shiny.
7, the tin furnace wave crest is unstable
8. The solder in the tin furnace contains impurities
9. Poor wiring direction and arrangement of components
10. Improper handling of the leads of the original bottom plate
5. No-clean flux picture